የኒኬል ደረጃ | ኒ+ኮ | Cu | Si | Mn | C | Cr | S | Fe | Mg |
≥ | ≤ | ||||||||
ኒ201 | ባል. | .25 | .3 | .35 | .02 | .2 | .01 | .3 | - |
ኒ200 | ባል. | .25 | .3 | .35 | .15 | .2 | .01 | .3 | - |
ቅይጥ | መደበኛ ስትራንድ ግንባታ, ሚሜ | መቋቋም፣Ω/ሜ | የስትራንድ ዲያሜትር ስም፣ ሚሜ | ሜትር በኪሎ |
NiCr 80/20 | 18×0.544+1×0.574 | 0.252-0.278 | 2.67 | 26 |
NiCr 80/20 | 19×0.61 | 0.205-0.250 | 3.05 | |
NiCr 80/20 | 18×0.523+1×0.574 | 0.271-0.299 | 2.67 | 30 |
NiCr 80/20 | 19×0.574 | 0.227-0.251 | 2.87 | 25 |
NiCr 80/20 | 36×0.385+1×0.45 | 0.265-0.293 | 2.76 | 26 |
NiCr 60/15 | 19×0.508 | 0.286-0.318 | 2.54 | |
NiCr 60/15 | 18×0.523+1×0.574 | 0.276-0.305 | 2.76 | 30 |
Ni200/Ni201 | 19×0.574 | 0.019-0.021 | 2.87 | 21 |
N6 | Chromel C፣ Ni 60፣ N6፣ HAI-NiCr 60፣ Tophet C፣ Resistohm 60፣ Cronifer II፣ |
ኤሌክትሮይ፣ ኒክሮም፣ አሎይ ሲ፣ ኒ 6፣ MWS-675፣ Stablohm 675 | |
N7 | ኒ 70፣ Chromel 70/30፣ N7፣ Hytemco፣ HAI-NiCr 70፣ Balco፣ Tophet 30፣ |
Resistohm 70፣ Cronix 70፣ Stablohm 710 | |
N8 | Chromel A፣ Ni 80፣ N8፣ Nichrome V፣ HAI-NiCr 80፣ Tophet A፣ Resistohm |
80፣ ክሮኒክስ 80፣ ፕሮቶሎይ፣ ኒ 8፣ አሎይ A፣ MWS-650፣ ስታብሎህም 650 |
ንብረቶች/ደረጃ | Cr20Ni80 | Cr30Ni70 | Cr15Ni60 | Cr20Ni35 | Cr20Ni30 | |
ዋና ኬሚካላዊ ቅንብር | Ni | እረፍት | እረፍት | 55.0-61.0 | 34.0-37.0 | 30.0-34.0 |
Cr | 20.0-23.0 | 28.0-31.0 | 15.0-18.0 | 18.0-21.0 | 18.0-21.0 | |
Fe | ≤ 1.0 | ≤ 1.0 | እረፍት | እረፍት | እረፍት | |
ከፍተኛ. የማያቋርጥ የአገልግሎት ሙቀት. የንጥረ ነገር | 1200 | 1250 | 1150 | 1100 | 1100 | |
የመቋቋም ችሎታ በ20 oC (μ Ω · ሜትር) | 1.09 | 1.18 | 1.12 | 1.04 | 1.04 | |
ትፍገት (ግ/ሴሜ 3) | 8.4 | 8.1 | 8.2 | 7.9 | 7.9 | |
የሙቀት ማስተላለፊያ (ኪጄ/ሜ · h · oC) | 60.3 | 45.2 | 45.2 | 43.8 | 43.8 | |
የመስመሮች መስፋፋት ጥምርታ (α × 10-6/ oC) | 18 | 17 | 17 | 19 | 19 | |
የማቅለጫ ነጥብ (በግምት)( oC) | 1400 | 1380 | 1390 | 1390 | 1390 | |
ሲሰበር ማራዘም (%) | > 20 | > 20 | > 20 | > 20 | > 20 | |
የማይክሮግራፊክ መዋቅር | ኦስቲኔት | ኦስቲኔት | ኦስቲኔት | ኦስቲኔት | ኦስቲኔት | |
መግነጢሳዊ ባህሪያት | መግነጢሳዊ ያልሆነ | መግነጢሳዊ ያልሆነ | መግነጢሳዊ ያልሆነ | መግነጢሳዊ ያልሆነ | መግነጢሳዊ ያልሆነ |